A Think Again Media Group publication
Science Debunk

Old window glass and its uneven thickness

Old window glass: the furnace marks and the flow calculation

By Phil Springer, Editor · Published · Science Debunk

Old window glass: the furnace marks and the flow calculation

The uneven thickness of old window glass begins with manufacturing methods that did not produce a uniformly flat sheet. The Victoria and Albert Museum describes a particularly revealing example: crown glass started as a hollow bubble, then became a spinning disc with a thick centre and thinner edges. The gradient existed before a glazier cut the material into window pieces. Centuries of installation were unnecessary to create it. A separate calculation using a medieval glass composition also puts room-temperature movement on a scale far smaller than a visible sag or ripple.

Crown production required several changes of shape. A glassmaker transferred the bubble from a blowpipe to a metal rod called a pontil, opened it, and spun it until centrifugal forces flattened it. The alternative broad-sheet method began with a bubble worked into a cylinder. That cylinder was slit lengthwise, reheated, and pressed into a sheet. Both routes shaped hot material by hand. The V&A's historical description also distinguishes the glassmaker from the painter: stained-glass painters commonly purchased sheets through merchants connected to glasshouses. A finished window therefore combined material made elsewhere with the glazier's cutting, painting, and assembly.

One surviving object gives those stages a specific setting. The V&A holds a German panel depicting the Entry into Jerusalem, dated about 1375 and catalogued as C.200-1912. It came from the choir windows of Erfurt Cathedral and formed part of a Passion scene. The museum's description of its reproduction identifies a full-size drawing called a cartoon, solid pieces of coloured glass cut to shape, enamel decoration, and lead strips joining the pieces. The museum identifies its reconstruction with a specific object, subject, and place of origin. Its description follows solid glass through cutting and decoration before the pieces become a joined image. A leaded panel is an assembly of individually prepared pieces, rather than a single transparent slab.

The distinction matters when old window glass changes shape after installation. The National Park Service identifies glass, metal cames, putty, the surrounding frame, and the environment as separate components of a stained-glass window. Its preservation guidance describes handblown material as unevenly textured, in contrast with more evenly textured machine-rolled glass. It also documents deterioration of cames and frames, cracking, and bulging. A window can therefore suffer genuine structural movement. That movement involves an assembly with metal joints and supports; a bulging panel and a thickness gradient within one piece are different physical features.

Putty supplies one route to later movement. The Park Service describes it hardening and cracking, losing adhesion between glass and came, and allowing individual pieces to rattle. Moisture can pit or etch glass and erode metal. Temperature changes make leaded glass expand and contract, loosening or breaking solder joints; inadequately supported windows can buckle under their own weight. These are documented changes in the condition of an installed window. They involve joints, surfaces, and supports, distinct from the original thickness variations of old window glass cut from a handmade sheet.

For the glass material itself, Ozgur Gulbiten, John Mauro, Xiaoju Guo, and Olus Boratav investigated a composition typical of the medieval glazing at Westminster Abbey. Their study appeared in the Journal of the American Ceramic Society in January 2018. They incorporated thermal history into the calculation because the material's earlier heating and cooling affect its subsequent behaviour. The estimated room-temperature viscosity was roughly 10^24 to 10^25 pascal-seconds. That was about 16 orders of magnitude below an earlier estimate for soda-lime-silicate glass. Lower viscosity still left an enormous resistance to flow.

Using analytical expressions for glass moving over a wall, the team calculated a maximum displacement of approximately one nanometre in a billion years. That is a model result for the investigated composition and thermal histories, rather than a time-lapse measurement of a cathedral pane. Even the revised estimate allowed no measurable viscous flow over human timescales. Old window glass can preserve variations produced in the hot workshop without having acquired them through a slow migration toward the sill.

An original industrial document shows how deliberately later manufacturers tackled surface defects. US patent 2,911,759, granted in 1959 to Lionel Pilkington and Kenneth Bickerstaff, describes a continuous glass ribbon supported on molten metal. Its specification discusses irregularities introduced by sizing rolls and supports, then a controlled heating stage intended to remove undulations while the ribbon floats. The glass is subsequently cooled enough for mechanical transport. The patent concerns active thermal treatment during manufacture. Together with the older crown and cylinder methods, it locates the creation and correction of uneven surfaces at the furnace, where temperature and forming equipment determine the finished sheet.

The Question

Why can an old window pane be thicker at the bottom than at the top?

Show the answer

The Answer

Historical manufacturing methods produced panes with uneven thickness. Ordinary glass is an amorphous solid, and the sags and ripples in old panes were present when they were made.