The resin with more than one stage

Baekeland's Bakelite and the problem of permanent form

By Phil Springer, Editor · Published · Science Debunk

Baekeland's Bakelite and the problem of permanent form

Baekeland's Bakelite had a distinction built into its earliest technical descriptions: the workable intermediate and the hardened final substance were different stages. Leo Hendrik Baekeland's U.S. patent 942,699, granted on December 7, 1909, described its final phenol-formaldehyde product as hard, insoluble, and infusible. The last property meant that the finished material did not melt back into a liquid. The American Chemical Society classifies Bakelite as a thermosetting resin and records that its molded form remained set when heated again.

Baekeland arrived at synthetic resins after an earlier commercial success. The Science History Institute records his doctorate at Ghent, a period of teaching, and a fellowship journey to New York in 1889. Charles F. Chandler encouraged him to remain in the United States. His subsequent work in photographic materials produced Velox, a paper developed under artificial light. Eastman Kodak purchased the invention in 1899. That transaction preceded his search for a synthetic resin, which he described as a deliberate business choice rather than an accidental diversion.

His initial objective was a substitute for shellac. According to the Institute's biography, his investigations of phenol and formaldehyde first yielded a soluble resin called Novolak, which failed to become a market success. His work then turned toward a binder associated with molded materials. The successful plastic dates to 1907 in the Institute's account. That history separates a commercial aim, an unsuccessful early product, and the later material named for its inventor. The name Bakelite did not erase the differences among the substances encountered along the way.

The American Chemical Society's history reproduces laboratory notes in which Baekeland assigned letters to products. One entry distinguished A, B, C, and D; the last was described as insoluble and unable to soften. He later treated C and D as equivalent. The lettering recorded changing physical properties within the investigation. These entries accompanied the development of Baekeland's Bakelite before his public announcement to the New York section of the Society on February 8, 1909. The laboratory distinctions preceded the material's broader commercial identity.

Patent 942,699 set out some of those distinctions in technical language. It described an initial oily material and another material with a viscous, gelatinous, or partly plastic consistency. Their behavior in solvents differed from that of the final hard substance. Baekeland characterized the finished product through resistance to moisture and ordinary chemical reagents as well as its inability to fuse. He compared a compact finished mass with hard rubber or ivory. These were claims about the result of a chemical transformation, rather than a description of unchanged material alternating between liquid and solid.

The same patent covered a range of compositions. Its descriptions included the resin by itself and compounds containing fibrous or powdered materials. Wood fiber, mica, mineral powders, and coloring substances appeared among its examples. It also distinguished molded pieces from blocks or irregular masses subsequently worked into shape. The finished product's infusibility coexisted with this variety of forms and ingredients. Baekeland's Bakelite was therefore represented in the patent as a family of manufactured compositions sharing a hardened resin, rather than one standardized object with a single appearance.

A second patent extended the manufacturing history of Baekeland's Bakelite beyond the first announcement. U.S. patent 1,160,362, filed on October 2, 1909, and granted on November 16, 1915, named General Bakelite Company as the assignee. It described difficulties in the existing molding materials, including pasty mixtures that were awkward to handle and dry mixtures that occupied considerable volume. The document proposed paper-like molding stock as a commercial alternative. Its account retained the distinction between partial reaction products and the final hard, infusible substance while addressing storage, transport, and consistency in production.

The products envisaged in that specification ranged from buttons and handles to trays, boxes, furniture, and musical instruments. Its use of the term paper encompassed thin sheets, cardboard, and pulp-board. It also discussed differing colors and appearances, including marbled and mottled effects. Those passages recorded an ambition to supply varied finished goods from related materials. They did not describe the final objects as repeatedly meltable. The same document identified the higher stages of condensation with infusibility, preserving the physical distinction that had appeared in the earlier patent.

Commercial production expanded around these developments. The American Chemical Society records the formation of a U.S. company in 1910, after laboratory production had reached about 180 liters daily, chiefly for electrical insulators. By 1930, the Bakelite Corporation occupied a 128-acre plant at Bound Brook, New Jersey. The company's infinity emblem and its slogan, The Material of a Thousand Uses, accompanied that expansion. In 1939, Baekeland retired and sold the company to Union Carbide and Carbon Corporation, according to the Science History Institute.

True or False?

Fully hardened Bakelite could be melted again and remolded.

Show the answer

The Record

Fully hardened Bakelite was infusible: it did not melt back into a moldable liquid. Baekeland's patents distinguished the workable intermediate products from the hard final material, which the American Chemical Society identifies as a thermosetting resin.